英文:Corrosion of reduced activation ferritic martensitic steel JLF-1 in purified Flinak at static and flowing conditions 
著者
和文: 近藤 正聡, 長坂 琢也, Valentyn TSISAR, 相良 明男, 室賀 健夫, Takashi WATANABE, 大島 智子, Yukihiro YOKOYAMA, Hiroshi MIYAMOTO, Eiji NAKAMURA, Naoki FUJII.  
英文: Masatoshi KONDO, Takuya NAGASAKA, Valentyn TSISAR, Akio SAGARA, Takeo MUROGA, Takashi WATANABE, Tomoko OSHIMA, Yukihiro YOKOYAMA, Hiroshi MIYAMOTO, Eiji NAKAMURA, Naoki FUJII.  
言語 English 
掲載誌/書名
和文: 
英文:Fusion Engineering and Design 
巻, 号, ページ Vol. 85        pp. 7-9
出版年月 2010年3月31日 
出版者
和文: 
英文:Elsevier 
会議名称
和文: 
英文: 
開催地
和文: 
英文: 
DOI https://doi.org/10.1016/j.fusengdes.2010.03.064
アブストラクト Flinak (LiF–KF–NaF) has the potential to be a tritium breeder candidate for a self-cooled fusion blan-ket or a secondary heat-transfer fluid of the blanket system. Corrosion of the structural material in Flinak is one of its issues. A corrosion test for Reduced Activation Ferritic Martensitic (RAFM) steel, JLF-1 (Fe–9Cr–2W–0.1C), was performed at 600 ◦ C using both purified and non-purified Flinak. The Flinak was purified by the electro-refining process, where Ni and H2O content in the Flinak were decreased. The test was performed at static conditions and flowing conditions induced by an impeller. The results of the test in non-purified Flinak showed local corrosion on the steel surface at the grain, packet, block and lath boundaries. The corrosion of JLF-1 in purified Flinak was much less than that in the non-purified Flinak. The corrosion in these boundaries was not severe, though pitting corrosion by the local electro-circuit was partly detected. This is due to local impurity condensation either in the Flinak or on the surface. The corrosion loss in flowing condition was small, the same as that in the static conditions. The number of pitting corrosions on the surface for flowing conditions was less than that in the static test. The occur-rence of pitting corrosion was controlled by the mixture and Flinak flow, in which the local impurity condensation was removed.